References | Author | Size (Substrate) | Frequency (MHz) | Sensitvity | Temperature compensation |
---|---|---|---|---|---|
[10] | Kurosawa et al. | - (128° LiNbO3) | 15 | - | No |
[11] | Varadan et al. | 1 × 1 mm2 (128° LiNbO3) | 74.2 | 705 μv/deg/s | No |
[12] | Wang et al. | 1.2 × 0.75 mm2 (128° LiNbO3) | 80 | 119 Hz/deg/s | Yes |
[14] | Oh et al. | 1.2 × 0.8 mm2 (128° LiNbO3) | 80 | 1.23 deg/deg/s | Yes |