Fig. 25From: High speed silicon wet anisotropic etching for applications in bulk micromachining: a reviewEtch rate and surface roughness of Si{100} as a function of (NH4)2S2O8 concentration in 10 wt% TMAH with dissolved 3.2 wt% silicon at 85 °C [106], © 2001, ElsevierBack to article page