Table 2 Design and electrodeposition conditions of the samples as a function of the OAR

From: Effects of a micro pattern on Cu alloy electrodeposition and its application as an oil detector

Open area ratio (%)

100

80

60

40

20

Pattern width (μm)

5

13.3

30

80

Applied current (mA)

50

40

30

20

10

Applied current density (mA/cm2)

50